Differential scanning calorimeter

TA Instruments DSC Q2000

DSC2Technical features

Temperature range: -90°C to 550°C
Temperature Accuracy: +/- 0.1°C
Temperature Precision: +/- 0.01°C
Calorimetric Reproducibility (indium metal): +/- 0.05%
Calorimetric Precision (indium metal): +/- 0.05%
Dynamic Measurement Range: >+/- 500 mW
Baseline Curvature (Tzero; -50 to 300˚C): 10 μW
Baseline Reproducibility with Tzero: +/- 10 μW
Sensitivity: 0.2 μW
Indium peak Height/Width: 60 mW/°C

Applications

Organic compounds, polymers and pharmaceuticals.

 